Machine tool ways have been made from cast iron on cast iron, from bronze on steel, and — since the 1960s — from a bonded PTFE-based liner on cast iron. Each has a place. The question is not which material is best in general, but which one suits the machine being rebuilt and the rework you are prepared to do.
The three options at a glance
| Aspect | PTFE-based liner | Bronze | Cast iron on cast iron |
|---|---|---|---|
| Friction at low speed | Low, and stays low — the reason stick-slip is reduced | Higher; prone to stick-slip when lubrication is marginal | Highest; depends entirely on the oil film |
| Wear part | The liner, which is renewable | The bronze facing, which must be re-fitted | The bed itself |
| Rework when clearance is lost | Strip and re-bond a new liner | Re-scrape or replace the bronze | Re-scrape or re-machine the casting |
| Lubrication demand | Tolerant of intermittent lubrication | Needs a reliable oil film | Needs a reliable oil film |
| Load capacity | Suited to slideway loads when sized correctly | High, and well understood on older machines | High |
| Best fit | Rebuilds where the bed is sound and the slide is worn | Heavy sliding loads on older designs | Original builds, lightly loaded axes |
Where the liner is clearly the better answer
- The bed is sound but the slide has worn and the clearance cannot be adjusted any further.
- The machine suffers stick-slip at low feed and the lubrication system has already been checked.
- A repeatable repair is wanted: the same liner thickness restores the same geometry each time.
- Downtime matters more than material cost — re-bonding is faster than re-scraping a casting.
Where it is not
If the bed itself is worn or distorted, a liner only moves the problem: the new layer follows the worn shape. In that case the way has to be machined or scraped first, and the liner is fitted afterwards. Very high specific loads on a narrow contact also need the section checked rather than assumed.
What changes after a conversion
Three things change when a worn bronze or iron slide is converted to a bonded liner. The friction at low feed drops, so the axis holds a slow move without stepping. The wear moves into a part that can be replaced without machining the bed. And the geometry becomes repeatable: the same liner thickness restores the same clearance, which makes the next rebuild predictable instead of a re-measurement exercise.
What does not change is the need for a sound bed. A liner follows the surface it is bonded to, so a twisted or hollow way transfers that error straight through the new layer. Machining or scraping comes first; the liner is the last operation, not the first.
In practice most conversions use a standard sheet for the slide and a two-part epoxy for the bond, with the finished thickness set by the machining allowance rather than by the sheet as supplied.
Why the grade matters more than the brand name
Rebuilders often ask for a material by trade name. What actually determines behaviour is the compound and the thickness. TEBAK supplies a PTFE-based replacement liner in four colours; each is listed with its own width and thickness values, and the colour guide sets out which grade is intended for which duty. Read that before comparing suppliers on price alone.
Comparing quotations properly
- Compare the same thickness and width — a lower price often means a thinner sheet.
- Check whether the bonding side is etched, and on which face.
- Ask what the price includes: cut sizes, packing by machine, or full sheets only.
- Confirm the adhesive is quoted with the liner, since it is consumed at the same time.
The sheet category lists the stock sizes, and the price guide explains what drives the cost so quotations can be compared line by line.
Tell us the machine and the wear measured on the ways, and we will say whether a liner alone is sufficient or the way needs machining first — through the quotation form.