A slide that moves in steps instead of gliding is showing stick-slip. The usual reflex is to adjust the control loop, but on a worn machine the cause is often mechanical: the sliding pair has reached a friction condition where static friction is much higher than kinetic friction. Re-lining fixes that. Adjusting the servo does not.
Wiper replacement is cheap; the wear it prevents is not. Check the wiper lip for hardening rather than for visible damage — a wiper that has gone hard looks intact but no longer seals, and the first sign is usually a polished band at one end of the travel rather than a chip.
The same applies to the way covers. A torn cover lets coolant and swarf onto the way, and the damage appears where the cover fails, not where the work is heaviest. Replacing covers on schedule costs far less than the localised wear they prevent.
What stick-slip actually is
At very low feed rates the slide stops, the drive builds force, the slide breaks free and overshoots, then stops again. The result is a visible ripple on the surface and a feed axis that will not hold a slow, steady move. Because the effect appears at low speed and disappears at high speed, it is often mistaken for a tuning problem.
Three conditions that produce the same symptom
- Friction condition — dry or contaminated way surfaces, or a worn liner with the low-friction layer gone.
- Backlash — lost motion in the screw, nut or thrust bearing, which shows as a step when the axis reverses.
- Geometric error — a way that is twisted or worn unevenly, so the slide tightens at one end of the travel.
Checks that isolate the cause
| Check | How | What it tells you |
|---|---|---|
| Low-feed behaviour | Command a slow move in one direction only | Ripple or judder in one direction points to friction, not backlash |
| Reversal step | Measure the step when the axis reverses | A step at reversal only is backlash |
| Lubrication | Check delivery at both ends of the travel | Dry patches or blocked metering units explain local sticking |
| Wear measurement | Measure the way along its length | Uneven wear changes clearance and loads one end harder |
| Contact pattern | Blue the slide and check the pattern | Patchy contact concentrates load and promotes local stick-slip |
Note: If the step only appears on reversal, stop here — that is backlash, not friction, and a new liner will not remove it.
When re-lining is the right answer
Re-lining is the correct fix when the contact pattern is patchy, the wear measurement shows the clearance has opened up, and the surface no longer holds lubricant. In that condition the liner is doing the work the original bearing surface can no longer do: it puts a renewable low-friction layer back between the slide and the bed.
The distinction matters commercially. A liner is a consumable with a known lead time; a control retune costs nothing but does not change the friction condition. If the same symptom has been tuned out twice and come back, the sliding pair is the more likely cause than the loop.
Choose the grade and size from the recorded specification rather than from habit — the blue sheet lists the stock widths and thicknesses, and the colour guide explains what each grade is for. Bonding consumes adhesive at the same time, so the two-part epoxy is normally ordered with the liner rather than after it.
What to record before ordering
- The measured wear at both ends of the travel
- The finished thickness you need after machining or scraping
- The way width, so the strip width follows the contact area rather than the machine size
- Whether the problem appeared after a rebuild, which points at bonding or clearance rather than material choice
Measure first with the wear measurement guide; if the pattern is patchy, the contact pattern note explains how to read it before you cut anything.